Diamond Series
PRODUCT SPECIFICATIONS |
DIAMOND 30 |
---|---|
Thickness of Film (Mil) | 3 |
Visible Light Transmission (VLT) | 30% |
Ultra Violet Rejection (UVR) 100nm-400nm | 100% |
HEV Blue Light Rejection (BLR) 380nm-420nm | 99% |
Infrared Light Rejection (IRR) 1400nm | 99% |
Total Solar Energy Rejection (TSER) | 80% |
Visible Light Reflectance (Inside) | 16% |
Visible Light Reflectance (Outside) | 19% |
Product Warranty (Indoor) | 10 Years |
Performance Warranty (IRR & UVR) | 10 Years |